Robusta LR은 충격 강도 및 연신율 측면에서 Robust G만큼 강하지는 않지만 인장 강도 및 굴곡 탄성률은 Robusta LR이 높고 열 성능은 Robusta G보다 우수하며 출력 정밀도가 더 높습니다.
| Measurement | Condition | Value |
|---|---|---|
| Viscosity | @ 26 °C (78.8 °F) | 450-520 cps |
| Color | White | |
| Density | @ 25 °C (77 °F) | 1.12 g/cm³ |
| Ec(critical exposure) | Dp(slop of cure-depth vs.ln(E) curve) |
|---|---|
| 8.5-9.3 mJ/cm2 | 0.125-0.14 |
| ASTM Method | Property Description | Value |
|---|---|---|
| ASTM D 638 | Tensile Modulus | 2540-2720 MPa |
| ASTM D 638 | Tensile Strength at Break | 45-53 MPa |
| ASTM D 638 | Elongation at Break | 7-10% |
| ASTM D 648 @66PSI | Heat Deflection Tempertature | 50-55℃ |
| ASTM D 790 | Flexural Strength | 60-75Mpa |
| ASTM D 790 | Flexural Modulus | 2080-2350Mpa |
| ASTM D 256 | Izod Impact (Notched) | 20-30 J/m |
| ASTM D 2240 | Hardness Shore D | 81-85 |